| ISO | AISI | DIN | PN |
| A2 | 304 | 1.4304 | OH18N9 |
| A4 | 316 | 1.4401 | OH17N12M2 |
| A4 | 316L | 1.4436 | OH17N12M3 |
| Klasa | 50 | 70 | 80 | 88 | 100/109 |
| Rm[MPa] | 500 | 700 | 800 | 800 | 1000 |
| Re0,2[MPa] | 210 | 450 | 600 | 640 | 900 |
| Stal/powłoka | Atm. przemysłowa |
Atm. morska |
| Powłoka cynkowa 1 |
2,5 roku | 5 lat |
| Powłoka cynkowa 2 |
15 lat | 30 lat |
| A2 | 25 lat | 50 lat |
| A4 | 50 lat | 100 lat |
| Klasa 80 | Klasa 70 | Klasa 50 |
| M5 | M6 | M9 |
| M6 | M8 | M10 |
| M8 | M11 | M14 |
| M10 | M12 | M18 |
| M12 | M16 | M20 |
| M16 | M20 | M27 |
| M20 | M24 | M33 |
| M24 | M30 | M42 |
| M30 | M36 | M52 |
| M36 | M45 | M60 |